VikingPyrotechnics Posted November 4, 2013 Share Posted November 4, 2013 Wanted to test my new star. There are metallic green + 7% sponge Ti The shell was not the best (not carefully constructed, because I only wanted to see my stars ) I think 5% Ti would be quite sufficient.?! https://www.youtube.com/watch?v=JAMjSrO0pE4 Greets VP Link to comment Share on other sites More sharing options...
leedrill Posted November 4, 2013 Share Posted November 4, 2013 awesome vp i agree less ti would be good not that 7% ruined it looked amazing for a quick shell did you use a winokur as a delay again in this one dosnt look like a glitter but very nice im jealous of your tails Link to comment Share on other sites More sharing options...
VikingPyrotechnics Posted November 4, 2013 Author Share Posted November 4, 2013 Thank you lee Yes, for the tail i pressed win39 for the delay .... This time it was milled for 3 hours or so Greets Link to comment Share on other sites More sharing options...
psyco_1322 Posted November 5, 2013 Share Posted November 5, 2013 (edited) VP, the stars in these shells had 5% spherical Ti. You can see how the Ti did not really show all that much in the red, but it did in the green. https://www.youtube.com/watch?v=XcH7EWDqq6I Your "throw together" shell came out looking pretty good. Edited November 5, 2013 by psyco_1322 Link to comment Share on other sites More sharing options...
VikingPyrotechnics Posted November 5, 2013 Author Share Posted November 5, 2013 Nice Shells ! Yes, i also had a batch of red stars ( ruby red ) with 5% sperical TI, and it was the same result as your?! Now i made a new batch with sponge TI and hope that it will be better Link to comment Share on other sites More sharing options...
Recommended Posts