kleberrios Posted August 15, 2013 Share Posted August 15, 2013 7030 magnalium is very hard to grind, but my home made shredder work well and grind 300 kg of 7030 magnalium very well http://www.youtube.com/watch?v=EmHuCs5RAKw&feature=youtu.be Link to comment Share on other sites More sharing options...
leedrill Posted August 15, 2013 Share Posted August 15, 2013 well done kleberrios looks like you have quite the little money machine there may i ask what you use for the next stage of processing Link to comment Share on other sites More sharing options...
FlaMtnBkr Posted August 15, 2013 Share Posted August 15, 2013 What do you use that ratio alloy for? Usually, I see 50:50 called for. Link to comment Share on other sites More sharing options...
kleberrios Posted August 15, 2013 Author Share Posted August 15, 2013 (edited) well done kleberrios looks like you have quite the little money machine there may i ask what you use for the next stage of processing Galga mill http://img.geocachin...56ca94c0dce.jpg http://mw2.google.co...ll/86935803.jpg http://1.bp.blogspot.com/_kIJ8HE_uKug/Sxegjc4umvI/AAAAAAAADgQ/AAbQMQHg7WM/s400/Duarte_Ferreira.jpg Edited August 15, 2013 by kleberrios Link to comment Share on other sites More sharing options...
kleberrios Posted August 15, 2013 Author Share Posted August 15, 2013 (edited) What do you use that ratio alloy for? Usually, I see 50:50 called for. This alloy burn faster and the red light is deeper. Flash powder, crossets, fish stars, hand red flare, fuse colored, report color become better. But no crackling, no strobe.... Edited August 15, 2013 by kleberrios Link to comment Share on other sites More sharing options...
mikeee Posted August 16, 2013 Share Posted August 16, 2013 Nice shredder!!! Link to comment Share on other sites More sharing options...