KAP Posted December 3, 2006 Share Posted December 3, 2006 Hi,David Blesser had some star formulas for magnesium and parlon. From what I make of it, there is no need for protecting the mag from corrosion? I havent used the potassium dichromate method for coating, I am a little chicken . Thanks, for the mortar tube info I will keep shooting as my tubes look fine. Kirk Link to comment Share on other sites More sharing options...
Mumbles Posted December 3, 2006 Share Posted December 3, 2006 As long as you use acetone to bind them you should be alright. For an extra degree of safety, you could dry your acetone. CaCl2, CaSO4, or Na2SO4 would all be acceptable to dry it. There are more, but those are rather OTC items. Link to comment Share on other sites More sharing options...
Mumbles Posted December 5, 2006 Share Posted December 5, 2006 Keep us posted if you try them. Post them in the Composition section with your comments if you would be so kind after you get a chance to test. Link to comment Share on other sites More sharing options...