crysanthemum 6, with 25 percent meal.

55/33/7/5 k/c/s/d

 

crackle comp,

bismuth trioxide 25

copper oxide 22

atomized al 250# 18

magnalium 200# 20

bind with nc, wear ppe, this crackle comp will self confine in powder form if ignited ( it will smoulder first)

 

what do you use?

 