Bonny Posted August 17, 2007 Share Posted August 17, 2007 My first wheel.Made from a 12" paint mixing stick with 4-1/2" ID x 3" long drivers. Was supposed to go in 2 stages but all drivers lit at once.2- drivers filled with silver fountain mix2-drivers filled with whistle+5%Ti(that I don't think lit). Does iron oxide increase burn temp? I plan on using longer drivers in the future...Any help on improving is wanted and appreciated. Link to comment Share on other sites More sharing options...
frogy Posted August 17, 2007 Share Posted August 17, 2007 Nice wheel indeed Uncle John =) Hope to see you here more often... Link to comment Share on other sites More sharing options...