Cartmann Posted January 23, 2022 Share Posted January 23, 2022 D1 - Glitter formula + 10% extra Aluminum Atomized Alcoa 120 A little to low. Wouldn't fit in a 1.91 mortar had to use a 2 inch. The shell could have used some booster. Thank for watching cartmann Link to comment Share on other sites More sharing options...
Carbon796 Posted January 23, 2022 Share Posted January 23, 2022 Not that it looks bad, but it does look like something is off with it. The shell vid, doesn't look like it really glitters at all. The comet vid has some glittering. But the tail looks really short. And the head is much brighter than I would expect. Like its using some of the aluminum for fuel. Rather than producing semi-reacted dross. Link to comment Share on other sites More sharing options...
Cartmann Posted January 24, 2022 Author Share Posted January 24, 2022 You are right that it looks off. I forgot to blade mill the sodium bicarbonate. Oops!! Link to comment Share on other sites More sharing options...