super nice !

:)

Link to comment
Share on other sites

Yus, stars were 14mm. 5-8-11-13-14(mm)

Composition is my, but not my property, i would say any will do, but first you need exact burn times of each. Those compositions are more or less "standard" but tweked in many ways for our needs.

It is 8leyer gumed tape. In each half one row of stars. Burst charge is flash but not flash with bp cork.

On the end formulas are not so important. Important is proces, details, chemicals. You need a lot of testing to get and understand your own technic, but each one have potential, only need tweking.

Edited by zan89
  • Like 2
Link to comment
Share on other sites

They looked like they kinda came out of the middle of the shell.